Request a Quote
Materials Surface Customisation Applications Custom Development Quality & Compliance Resources About FAQ Contact Request a Quote
Home / Resources / Recycled leather vs PU

Comparison

Recycled leather fibre vs PU vs microfiber

7 min read · ChengTai Leather

The right choice comes down to three questions in your brief: does the product need a recycled-content claim, what hand feel is it judged on, and what test does it have to pass. Answer those in order and the shortlist usually makes itself.

At a glance

Recycled leather fibrePUMicrofiber
Hand feelClose to leather; dry, slightly warmUniform, can feel plasticSoft, suede-like
Tear strength4–4.5 kg — internal test, our seriesConfirm per product and test methodConfirm per product and test method
Recycled content51% pre-consumer leather fibre + 20% recycled polyesterPossible — confirm per productPossible — confirm per product
Edge finishingNeeds edge paintNeeds edge paintNeeds edge paint
CostMidLowMid to high

1. Does it need a recycled-content claim?

If yes, recycled leather fibre is the only one of the three that contains leather fibre and carries a documented percentage: 51% pre-consumer leather fibre plus 20% recycled polyester in our DL26 series, covered by GRS and SCS. PU and microfiber can contain recycled content, but it is product-specific — ask for the percentage and the certificate, not the brochure line.

2. What hand feel is it judged on?

Recycled leather fibre reads closest to leather: dry, slightly warm, with a formed surface. PU is uniform and takes print and embossing easily, but can read plastic. Microfiber has the softest, most suede-like drape of the three. Judge them in the colour and finish the product will actually use, not in a neutral swatch book.

3. What performance does it have to pass?

Our recycled fibre series tests at 4–4.5 kg tear on our internal method. Performance footwear often specifies 6 kg, and microfiber is available at higher tear values than our sheet. Ask for the value under your own test method — a general range is not a specification.

Where each one wins

Do not choose on hand feel alone. Ask for the tear value and the recycled content percentage first; those two numbers eliminate most of the shortlist.

Shortlist by project

What a trial looks like

Sampling runs from 30–50 yards per colour with a 15-day sample lead time; standard MOQ is 300 yards per colour. Send the application, target thickness and colour reference, and we will come back with the series, the test values and the certificates that apply.

Start with a specification.

Application · thickness · colour reference — we reply within one working day